Duenne Leistungsmodul-Bodenplatte: CNC-Pruefung von Senkungen, Nut und Montagebezug

CNC-Bearbeitungsfall fuer eine duenne Aluminium-Bodenplatte mit vier Senkbohrungen, unterer Nut, Kantenstufen und Montagekontrolle.

Zurück zu Fallstudien
Duenne Leistungsmodul-Bodenplatte: CNC-Pruefung von Senkungen, Nut und Montagebezug

Summary: This case reviews a thin aluminum base shell for a telecommunications power module. Four counterbored mounting holes, a lower slot feature and thin edge steps require careful support, deburring and assembly verification.

Duenne Leistungsmodul-Bodenplatte: CNC-Pruefung von Senkungen, Nut und Montagebezug

Sichtbare Zeichnungsdaten

The drawing shows a 6063-T5 aluminum bottom shell with fine blasting and clear anodizing. Visible dimensions include an overall length around 78.60 mm, a lower width around 62.60 mm, a 70 mm internal reference, four mounting holes and a lower slot or step feature. [Source: Customer-provided engineering drawing visible annotations]

Duenne Leistungsmodul-Bodenplatte: CNC-Pruefung von Senkungen, Nut und Montagebezug

Bauteilfunktion und Risiko

The part likely works as a base or cover interface in an electronics module. Flatness, hole position and edge quality matter because the part may contact another housing or fastener stack.

Thin sections can deform under clamping force. Counterbored holes need clean bottom surfaces and consistent chamfers. The lower slot must keep its position relative to the hole pattern.

Duenne Leistungsmodul-Bodenplatte: CNC-Pruefung von Senkungen, Nut und Montagebezug

Prozessroute

A controlled route is to finish the reference faces first, support the plate during pocket and slot machining, finish the counterbores, then deburr under magnification. Surface treatment should not hide burrs or damage hole edges.

Pruefschwerpunkte

Inspection should confirm overall size, counterbore quality, hole spacing, slot position, edge chamfer and surface finish. Whenever possible, checks should refer to the actual mating component.

FAQ

Q1: Why is a thin flat part not automatically easy?

Because clamping, cutting force and deburring can bend edges or affect local flatness.

Q2: Which relationship matters for assembly?

The relationship between the four mounting holes and the lower slot is important.

Q3: What should be confirmed before production?

Material, finish, tolerances, mating part, fastener type, quantity and inspection method.

Scannen Sie, um uns zu kontaktieren

Kontakt: Allen

E-Mail: shiziqiu@oemach.com

My whatsapp code

Allen WhatsApp QR-Code

Projekt starten

Sagen Sie uns, was Sie fertigen lassen möchten.

Teilen Sie uns Ihre Bauteilanforderungen mit. Unser Engineering-Team prüft sie und meldet sich mit den nächsten Schritten.

Für eine fundierte Prüfung benötigen wir:

  • Material und Stückzahl
  • Kritische Toleranzen
  • Oberfläche und gewünschter Liefertermin
Zeichnungen und ergänzende Dateien (optional) 0 von 10 Dateien

Für eine schnellere Prüfung fügen Sie eine PDF-Zeichnung und ein STEP/STP-Modell bei. Packen Sie bei Baugruppen alle referenzierten Teile und die Stückliste in ein gemeinsames Archiv.

Mit dem Absenden stimmen Sie zu, dass OEMach diese Angaben und hochgeladenen Dateien zur Beantwortung Ihrer Anfrage verwendet. Mehr in unserer Datenschutzerklärung.